Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 48.6 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 48.6 W/m-K

@Temperature 20.0 °C
337 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Latrobe CBS-600â„¢ VIM-VAR Carburizing Bearing and Gear Steel
CBS-600 VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. Double vacuum melting is employed to provide optimum tensile properties as well as describe..
Copyright © lookpolymers.com All Rights Reserved