Thermal Properties Metric English Comments
Thermal Conductivity 52.7 W/m-K

@Temperature 800 °C
366 BTU-in/hr-ft²-°F

@Temperature 1470 °F
ATI Wah Chang Nb/Nb Alloy FS-85
Information provided by ATI Wah Chang