Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 6.00 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 6.00 W/m-K

@Temperature 100 °C
41.6 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast AK 99 S Dense Refractory Brick
Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qu..
Thermal Conductivity 6.00 - 8.00 W/m-K

@Temperature 600 °C
41.6 - 55.5 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS SiC 90 D Moldable Refractory Material
Description: This material is supplied as a dry powder. It has to be mixed with clean water to the necessary consistency. Curas SiC 90 has a phosphate bond and especially meant for protection of bo..
Thermal Conductivity 6.00 W/m-K

@Temperature 1400 °C
41.6 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Gouda Vuurvast VIBRON 160 K Dense Vibrating Refractory Castable
Description: Vibron 160 K is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity and high abrasion resistance. The thermal shock resistance is excell..
Thermal Conductivity 6.00 W/m-K

@Temperature 100 °C
41.6 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast LP 100 Dense Refractory Brick
Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qual..