Thermal Properties Metric English Comments
Thermal Conductivity 0.900 - 1.10 W/m-K

@Temperature 600 °C
6.25 - 7.63 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 40 Moldable Refractory Material
Description: Because of special additions this type of moldable already has a reasonable strength at room temperature. It is used for a wide range of applications.Remarks: The stated chemical compos..
Thermal Conductivity 0.900 - 1.10 W/m-K

@Temperature 100 °C
6.25 - 7.63 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 60 S Moldable Refractory Material
Description: Because this material contains a high percentage of sillimanite, it has a very good thermal shock resistance together with a very good slag resistance. Therefore this material finds its..
Thermal Conductivity 0.900 - 1.10 W/m-K

@Temperature 200 °C
6.25 - 7.63 BTU-in/hr-ft²-°F

@Temperature 392 °F
Gouda Vuurvast GI 34 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.900 W/m-K

@Temperature 1100 °C
6.25 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Zircar Ceramics AX-200 Refractory Supported Heater
ZIRCAR Refractory Supported Heater Type AX-200 consists of high temperature, helically-wound, iron-chrome-aluminum metallic alloy resistance heating elements fully embedded in a strong, highly stabl..