Thermal Conductivity 0.970 - 1.17 W/m-K

@Temperature 600 °C
6.73 - 8.12 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 85 P Moldable Refractory Material
Description: This phosphate bonded material based on corundum and bauxite has already at low temperature a reasonable strength and has a very good resistance against slag attack or liquid aluminum. ..
Thermal Conductivity 0.970 - 1.17 W/m-K

@Temperature 600 °C
6.73 - 8.12 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 85 PD Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This phosphate bonded material based on corundum and bauxite has a very go..
Thermal Conductivity 0.970 - 1.17 W/m-K

@Temperature 600 °C
6.73 - 8.12 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 85 PD GM Moldable Refractory Material
Description: This material is supplied as a dry powder and can be gunned. This phosphate bonded material based on corundum and bauxite has a very good resistance against slag attack or liquid alumin..