Thermal Properties Metric English Comments
Thermal Conductivity 0.988 W/m-K

@Temperature 600 °C,
Time 10800 sec
6.86 BTU-in/hr-ft²-°F

@Temperature 1110 °F,
Time 3.00 hour
Sharadaa Ceramics REFCAST K High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Thermal Conductivity 0.988 W/m-K

@Temperature 600 °C,
Time 10800 sec
6.86 BTU-in/hr-ft²-°F

@Temperature 1110 °F,
Time 3.00 hour
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Thermal Conductivity 0.988 W/m-K

@Temperature 800 °C,
Time 10800 sec
6.86 BTU-in/hr-ft²-°F

@Temperature 1470 °F,
Time 3.00 hour
Sharadaa Ceramics REFCAST C High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..
Thermal Conductivity 0.988 W/m-K

@Temperature 600 °C,
Time 10800 sec
6.86 BTU-in/hr-ft²-°F

@Temperature 1110 °F,
Time 3.00 hour
Sharadaa Ceramics REFCAST C High Alumina Castables
Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr..