Thermal Properties Metric English Comments
Thermal Conductivity 5.00 - 7.00 W/m-K

@Temperature 1300 °C
34.7 - 48.6 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURAS SiC 70 D GM Moldable Refractory Material
Description: This gunning material is supplied as a dry powder. Curas SiC 70 D GM has a phosphate bond and is specially developed as a protection layer on boiler tubes.Remarks: The stated chemical c..
Thermal Conductivity 5.00 - 7.00 W/m-K

@Temperature 100 °C
34.7 - 48.6 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS SiC 90 D Moldable Refractory Material
Description: This material is supplied as a dry powder. It has to be mixed with clean water to the necessary consistency. Curas SiC 90 has a phosphate bond and especially meant for protection of bo..
Thermal Conductivity 5.00 - 7.00 W/m-K

@Temperature 1300 °C
34.7 - 48.6 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURAS SiC 70 D Moldable Refractory Material
Description: This material is supplied as a dry powder and has to be mixed with clean potable water to the necessary consistency. Curas SiC 70D has a phosphate bond and is specially developed for b..
Thermal Conductivity 5.00 - 7.00 W/m-K

@Temperature 100 °C
34.7 - 48.6 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast VIBRON 160 K 50 Dense Vibrating Refractory Castable
Description: Vibron 160 K 50 is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity, high abrasion resistance and a good oxidation resistance up to 1..