Thermal Conductivity 11.3 W/m-K

@Temperature 23.0 °C
78.4 BTU-in/hr-ft²-°F

@Temperature 73.4 °F
Carpenter Thermo-Span® Fe-Co-Ni Superalloy
Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h..