Thermal Properties Metric English Comments
Thermal Conductivity 120 W/m-K

@Temperature 25.0 °C
833 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Osprey Metals CE7 Al-Si Controlled Expansion Alloy
Si-30%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.
Thermal Conductivity 120 W/m-K

@Temperature 100 °C
833 BTU-in/hr-ft²-°F

@Temperature 212 °F
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Thermal Conductivity 120 W/m-K

@Temperature 20.0 - 100 °C
833 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
DIN EN 821-2 / ASTM-C408
CeramTec Rocar® SiF Silicon Carbide, SiSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..
Thermal Conductivity 120 W/m-K

@Temperature 20.0 °C
833 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
hardened to 30 HRC
Bohler-Uddeholm BeCu Alloy 172 Mold Material
Beryllium copper alloyA high strength beryllium copper mold alloy with high thermal conductivity.BeCu Alloy 172 is characterized by: High thermal conductivity Good corrosion resistance Good polisha..