Polymer Property : Thermal Conductivity = 87.4 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 12.6 W/m-K

@Temperature 200 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Waspaloyâ„¢ alloy, sheet
Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, go..
Thermal Conductivity 12.6 W/m-K

@Temperature 200 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 12.6 W/m-K

@Temperature 200 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 12.6 W/m-K

@Temperature 200 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 12.6 W/m-K

@Temperature 200 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 12.6 W/m-K

@Temperature 200 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 12.6 W/m-K

@Temperature 200 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 392 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 12.6 W/m-K

@Temperature 150 °C,
Time 3600 sec
87.4 BTU-in/hr-ft²-°F

@Temperature 302 °F,
Time 1.00 hour
Epoxy Technology EPO-TEK® EK1000 Epoxy
Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding ..
Thermal Conductivity 12.6 W/m-K

@Temperature 150 °C,
Time 3600 sec
87.4 BTU-in/hr-ft²-°F

@Temperature 302 °F,
Time 1.00 hour
Epoxy Technology EPO-TEK® EK1000-MP Epoxy
Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding ..
Thermal Conductivity 12.6 W/m-K

@Temperature 150 °C,
Time 3600 sec
87.4 BTU-in/hr-ft²-°F

@Temperature 302 °F,
Time 1.00 hour
Epoxy Technology EPO-TEK® EK2000 Epoxy
Preliminary Product Information SheetMaterial Description: A two component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance ..
Thermal Conductivity 12.6 W/m-K

@Temperature 204 °C
87.4 BTU-in/hr-ft²-°F

@Temperature 399 °F
ATI Allegheny Ludlum AL 625HP™ Stainless Steel
Nickel-based superalloy. Characteristics:exceptional fatigue resistance, excellent resistance to oxidation and corrosion, outstanding strength and toughness over a range of temperatures from cryogen..