Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 132.7 W/m-K @Temperature 100 °C |
920.9 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Thermal Conductivity | 132.7 W/m-K @Temperature 100 °C |
920.9 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T7 Heat Treatment Condition T7 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Thermal Conductivity | 132.7 W/m-K @Temperature 100 °C |
920.9 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T6 Heat Treatment Condition T6 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |