Thermal Properties Metric English Comments
Thermal Conductivity 13.5 W/m-K

@Temperature 300 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Thermal Conductivity 13.5 W/m-K

@Temperature 300 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Thermal Conductivity 13.5 W/m-K

@Temperature 100 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 13.5 W/m-K

@Temperature 100 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 13.5 W/m-K

@Temperature 100 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 13.5 W/m-K

@Temperature 100 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 13.5 W/m-K

@Temperature 100 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 13.5 W/m-K

@Temperature 100 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 13.5 W/m-K

@Temperature 100 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Thermal Conductivity 13.5 W/m-K

@Temperature 300 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Thermal Conductivity 13.5 W/m-K

@Temperature 300 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Thermal Conductivity 13.5 W/m-K

@Temperature 300 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Thermal Conductivity 13.5 W/m-K

@Temperature 100 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..
Thermal Conductivity 13.5 W/m-K

@Temperature 100 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..
Thermal Conductivity 13.5 W/m-K

@Temperature 300 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe..
Thermal Conductivity 13.5 W/m-K

@Temperature 300 °C
93.7 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe..
Copyright © lookpolymers.com All Rights Reserved