Thermal Properties Metric English Comments
Solidus 1010 °C
1850 °F
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; H (TD04) Temper; up to 76 mm Thickness (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Solidus 1010 °C
1850 °F
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; HT (TH04) Temper; up to 76 mm Thickness (UNS C17500)
Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Solidus 1010 °C
1850 °F
Materion Beryllium Copper Alloy 10 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Solidus 1010 °C
1850 °F
Materion Beryllium Copper Alloy 10 Rod and Bar; AT (TF00) Temper; All Sizes (UNS C17500)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Solidus 1010 °C
1850 °F
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17500)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Solidus 1010 °C
1850 °F
Materion Beryllium Copper Alloy 10 Rod and Bar; H (TD04) Temper; up to 76 mm (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Solidus 1010 °C
1850 °F
Materion Beryllium Copper Alloy 10 Rod and Bar; HT (TH04) Temper; up to 76 mm (UNS C17500)
Treatment required for max strength: 2 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Solidus 1010 °C
1850 °F
Materion Beryllium Copper Alloy 10 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Solidus 1010 °C
1850 °F
Materion Beryllium Copper Alloy 10 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: 3 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material..
Solidus 1010 °C
1850 °F
Materion Beryllium Copper Alloy 10 Wire; H (TD04) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Solidus 1010 °C
1850 °F
Materion Beryllium Copper Alloy 10 Wire; HT (TH04) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: 2 hrs @ 480-495°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material..
Solidus 1010 °C
1850 °F
Materion Beryllium Copper Alloy 10 Forgings & Extrusions; A (TB00) Temper (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Solidus 1010 °C
1850 °F
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Solidus 1010 °C
1850 °F
Materion Beryllium Copper Alloy 10 Forgings & Extrusions; AT (TF00) Temper (UNS C17500)
Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc...