Polymer Property : Solidus = 1155 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 623.9 °C
1155 °F
Melting Point
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
BR 616 strip coated with Ti for joining ceramics without metallization.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal strip in wrought Cerametil
Solidus 623.9 °C
1155 °F
Melting Point
Lucas-Milhaupt Lucanex 616 Active Metal Brazing
Brazing Paste Blended with Ti for active metal brazing of ceramics.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal powder in Lucanex paste
Solidus 623.9 °C
1155 °F
Melting Point
Lucas-Milhaupt Premabraze 616 Silver Based Cadmium Free Filler Metal
Applications: Application is found in all types of moderate temperature low pressure systems, and in particular the electronic vacuum tube. Characteristics:Premabraze 616 is a low temperature, sl..