Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 1329 °C
2424 °F
Kennametal Stellite Stellite® 25 Cobalt Chromium Cast Alloy
Stellite alloy 25 forms a protective oxide film during hot metal-on metal wear which prevents metal transfer and damage due to adhesion. The alloy is resistant to thermal cracking and surface fatig..