Thermal Properties Metric English Comments
Solidus 144 °C
291 °F
Indium Corp. Indalloy 86 Bismuth-Cadmium Solder Alloy
Information Provided by Indium Corporation
Solidus 144 °C
291 °F
Indium Corp. Indalloy® 97 Pb-Sn-Bi Solder Alloy
Good general purpose step soldering alloy.Information provided by the manufacturer, Indium Corporation.