Polymer Property : Solidus = 146 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 146 °C
295 °F
Indium Corp. Indalloy 102 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Solidus 146 °C
295 °F
AIM 97In/3Ag Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.