Polymer Property : Solidus = 150 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 150 °C
302 °F
Indium Corp. Indalloy 88 Indium Solder Alloy
Information Provided by Indium Corporation
Solidus 150 °C
302 °F
Johnson Matthey JM A-Core Soft Solder Flux
The standard "acid" flux core used for most industrial applications where an aggressive flux is required. Residues are corrosive.Information provided by Johnson Matthey.
Solidus 150 °C
302 °F
Johnson Matthey JM No1S Soft Solder Flux
A highly active liquid flux recommended for use on Stainless and carbon steels. Generally used with the Silver/Tin alloys such as JM P40 and JM P5. Residues are corrosive and should be removed aft..
Solidus 150 °C
302 °F
Johnson Matthey JM No2S Soft Solder Flux
A liquid non-corrosive flux for use on copper and brass. The residues are water soluble and non-corrosive, however it is recommended they are removed to prevent any possibility of contamination aft..
Solidus 150 °C
302 °F
Johnson Matthey JM PA Soft Solder Flux
PA flux is a highly active flux paste suitable for use on Stainless Steel in conjunction with the silver bearing soft solders. Like JM 1S the residues are corrosive and should be removed with water..
Solidus 150 °C
302 °F
Johnson Matthey JM R-Core Soft Solder Flux
A "rosin" type core generally used for joining copper and brass. Residues are non-corrosive.Information provided by Johnson Matthey.