Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Solidus = 1770 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 966 °C
1770 °F
Universal Wire Works BNi-2 (AMS 4777) Nickel Base Brazing Filler Metal
Information provided by Universal Wire Works for their line of welding wire and filler metal.
Solidus 966 °C
1770 °F
Universal Wire Works BNi-3 (AMS 4778) Nickel Base Brazing Filler Metal
Information provided by Universal Wire Works for their line of welding wire and filler metal.
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TB Quenched Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TB Quenched Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TD1 Quenched/Cold Rolled, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TD1 Quenched/Cold Rolled, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TD2 Quenched/Cold Rolled, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TD2 Quenched/Cold Rolled, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TD3 Quenched/Cold Rolled, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TD3 Quenched/Cold Rolled, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TD4 Quenched/Cold Rolled, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TD4 Quenched/Cold Rolled, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TDX Quenched/Cold Rolled, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TDX Quenched/Cold Rolled, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TF Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TF Quenched/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TH1 Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TH1 Quenched/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TH2 Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TH2 Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TH3 Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TH4 Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TH4 Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 TH3 Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 THX Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Solidus 968 °C
1770 °F
CLAL-MSX NICLAFOR® 1000 THX Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..