Polymer Property : Solidus = 226 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 108 °C
226 °F
Indium Corp. Indalloy® 224 In-Sn-Zn Solder Alloy
Pb free solder, high dross due to Zn.Information provided by the manufacturer, Indium Corporation.
Solidus 108 °C
226 °F
Indium Corp. Indalloy 61 Bismuth Solder Alloy
Information Provided by Indium Corporation