Polymer Property : Solidus = 235 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 235 °C
455 °F
Indium Corp. Indalloy® 133 Sn-Sb Solder Alloy
Higher tensile strength solder than #121. Particular application is joining copper tubing in refrigeration and potable water systems. Has good wettability with good long time sheer strength at 100Â..
Solidus 235 °C
455 °F
Williams Advanced Alloys WS235 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys