Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 1317 °C | 2403 °F | |
Special Metals INCONEL® alloy 693 INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t.. |