Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 1285 - 1350 °C
2345 - 2460 °F
Kennametal Stellite Denertiaâ„¢ C14 Cobalt Chromium Dental Alloy
Denertia™ C14 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework. It conforms to the following International Standards: EN 1641 §..