Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 304 °C | 579 °F | |
Indium Corp. Indalloy 229 Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 304 °C | 579 °F | |
Indium Corp. Indalloy® 237 Pb-Sn-Ag-In Solder Alloy High temp solder.Information provided by the manufacturer, Indium Corporation. |
|||
Solidus | 304 °C | 579 °F | |
Johnson Matthey JM A5 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |