Solidus 515.9 - 521.9 °C
960.6 - 971.4 °F
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6
Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo..
Solidus 515.9 - 521.9 °C
960.6 - 971.4 °F
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x
Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all..