Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 300 °C | 572 °F | |
Indium Corp. Indalloy 168 Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 300 °C | 572 °F | |
Indium Corp. Indalloy® 164 Pb-In-Ag Solder Alloy This alloy is very useful in the 300°C range. It has particularly good thermal fatigue properties as well as the minimal gold leaching properties of indium-lead alloys. Often used in reducing atm.. |
|||
Solidus | 300 °C | 572 °F | |
Indium Corp. Indalloy 11 Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 300 °C | 572 °F | |
Williams Advanced Alloys WS300 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 300 °C | 572 °F | |
Williams Advanced Alloys WS314 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |