Polymer Property : Solidus = 649 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 649 °C
1200 °F
Melting Point
Lucas-Milhaupt BRAZE 380
Characteristics:Braze 380 is a free-flowing, low temperature filler metal with excellent wetting of most ferrous and non-ferrous base metals, and is a good substitute for cadmium-bearing filler meta..
Solidus 649 °C
1200 °F
Lucas-Milhaupt Silvacore® A38T Flux Cored Brazing Alloy
Silvaloy A38T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult to wet metals..
Solidus 649 °C
1200 °F
Lucas-Milhaupt Silvaloy® A38T Brazing Alloy
Silvaloy A38T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult to wet metals..
Solidus 649 °C
1200 °F
Lucas-Milhaupt Silvaloy® A40T Brazing Alloy
Silvaloy A40T is a good general purpose, low melting, cadmium-free alloy, often selected for its low temperature, wetting and good flow. Silvaloy A40T has a lower brazing temperature with a relative..
Solidus 649 °C
1200 °F
Lucas-Milhaupt Silvacap 35490 Brazing Alloy
Silvacap is a low brazing temperature, cadmium-free alloy. It has a slight plastic range which may be noticed during melting on some applications. Generally, the joint strength using Silvacap will s..
Solidus 649 °C
1200 °F
Melting Point
Lucas-Milhaupt BRAZE 402 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 402 is a free-flowing, intermediate temperature filler metal and as such is a good substitute for cadmium-bearing filler metals with similar silver contents. The material is ..