Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Solidus = 80.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 80.0 °C
176 °F
Indium Corp. Indalloy 31 Bismuth Solder Alloy
Information Provided by Indium Corporation
Solidus 80.0 °C
176 °F
Indium Corp. Indalloy 32 Bismuth Solder Alloy
Information Provided by Indium Corporation
Copyright © lookpolymers.com All Rights Reserved