Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 820 °C | 1510 °F | |
Wieland 1023 Wilaform Gold Hard yellow gold alloy with good extensibility. Particularly suitable for by machine manufactured decoration.Applications: casting, chains, coin/shape, laminar decorationDental |
|||
Solidus | 820 °C | 1510 °F | |
Wieland 1101 Wilaform Gold Hard yellow gold alloy with good extensibility. Universally applicable in decoration manufacturing.Applications: casting, chainsDental |
|||
Solidus | 820 °C | 1510 °F | |
Wieland 1114 Wilaform Gold Hard yellow gold alloy with good extensibility. Universally applicable in decoration manufacturing.Applications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental |
|||
Solidus | 820 °C | 1510 °F | |
Wieland 3013 Wilaform Silver Universally applicable silver alloy.Applications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental |