Polymer Property : Liquidus = 1140 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 613 °C
1140 °F
PCC-Advanced Forming Technology 63% AlSiC Metal Matrix Composite
AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements ..
Liquidus 613 °C
1140 °F
PCC-Advanced Forming Technology 68% AlSiC Metal Matrix Composite
AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements ..
Liquidus 613 °C
1140 °F
PCC-Advanced Forming Technology 70% AlSiC Metal Matrix Composite
AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements ..
Liquidus 613 °C
1140 °F
PCC-Advanced Forming Technology AlSiC-SD Metal Matrix Composite
AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements ..
Liquidus 613 °C
1140 °F
Solvay Chemicals NOCOLOK® Braze Paste x43-7
A braze paste specifically formulated for providing viscous mixture of flux and alloy for brazing noncladded aluminum materials, including 1100, 3001 and 6061 series aluminum. Uses: Automotive Sect..