Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1315 °C | 2399 °F | |
Materion Beryllium Nickel M220C Information supplied by Brush Wellman Engineered Materials.Brush M220C is characterized by high levels of strength, hardness, and thermal conductivity combined with excellent resistance to wear, cor.. |