Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1320 °C | 2400 °F | |
IBC Advanced Alloys FA230 Beryllium Nickel Casting Alloy Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th.. |