Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, 0% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, 10% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, 10% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, 30% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, 50% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, all-weld metal, GMAW short arc HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, GTAW weld, C-22 base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, SMAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, SMAW weld, C-22 base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, transverse, GMAW short arc weldment, plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, transverse, GMAW spray weldment, 23.4 mm thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Liquidus | 1399 °C | 2550 °F | |
AK Steel 316L Austenitic Stainless steel AK Steel 316L is an extra-low carbon version of AK Steel 316 that minimizes harmful carbide precipitation due to welding.Information provided by AK Steel |
|||
Liquidus | 1399 °C | 2550 °F | |
AK Steel 321 Austenitic Stainless steel AK Steel 321 is a stabilized austenitic stainless steel similar to Type 304 but with a titanium addition. This titanium addition reduces or prevents carbide precipitation during welding and in 427 .. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, all-weld metal, SMAW HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, GMAW, as welded, notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, GMAW, as welded, unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, GTAW, as welded, unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, transverse, GTAW short arc weldment, plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, transverse, GTAW spray weldment, 12.7 mm (1/2 in.) thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, transverse, SMAW weldment, 19.1 mm thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, 60% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, GMAW, aged 4000 hours at 450°C (800°F), notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, GMAW, aged 4000 hours at 450°C (800°F), unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, GTAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Liquidus | 1399 °C | 2550 °F | |
Haynes Hastelloy® C-22® alloy, SMAW weld, 904L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |