Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Liquidus = 1685 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 918.3 °C
1685 °F
Flow Point
Lucas-Milhaupt HANDY HI-TEMP 548® Carbide Brazing Alloy
Applications: Handy Hi-Temp 548 is a modified nickel-silver filler metal primarily used to join tungsten carbide to steel. Brazing is often combined with heat treatment of the steel tool bits. The..