Polymer Property : Liquidus = 1750 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 955 °C
1750 °F
Materion Beryllium Copper Alloy 245C Castings (UNS C82600)
Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula..
Liquidus 955 °C
1750 °F
Materion Beryllium Copper Alloy 245CT Castings (UNS C82600)
Pouring Temperature: 970-1065°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchTabula..
Liquidus 955 °C
1750 °F
Williams Advanced Alloys Wambraze™ WB955 Solder
High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de..