Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 1040 °C | 1900 °F | |
Osprey Metals HTN 3 Brazing Powder Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requireme.. |
|||
Liquidus | 1040 °C | 1900 °F | |
Universal Wire Works BNi-2 (AMS 4777) Nickel Base Brazing Filler Metal Information provided by Universal Wire Works for their line of welding wire and filler metal. |
|||
Liquidus | 1040 °C | 1900 °F | |
Weartech International WT-60 Nickel Hardfacing & Wear Resistant Alloy Applications: pump sleevesInformation provided by Weartech International |
|||
Liquidus | 1040 °C | 1900 °F | |
Wieland 1701 Wilaform Gold Yield alloy particularly suitable for coin and medal production. Also can be welded into platinum suitably.Applications: coin/shapeDental |
|||
Liquidus | 1040 °C | 1900 °F | |
Wieland 1909 Wilaform Gold Hard palladium white gold alloy with beautiful white color.Applications: casting, chains, laminar decoration, pipes, tubingDental |