Polymer Property : Liquidus = 1960 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 1070 °C
1960 °F
Osprey Metals HTN 1A Brazing Powder
Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requireme..
Liquidus 1070 °C
1960 °F
Osprey Metals HTN 4 Brazing Powder
Particle size distribution 1-250 microns.SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requireme..
Liquidus 1070 °C
1960 °F
Materion Beryllium Copper Alloy 174 Strip; 1/2HT (TH02) Temper (UNS C17410)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 95%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R..
Liquidus 1070 °C
1960 °F
Materion Beryllium Copper Alloy 174 Strip; HT (TH04) Temper (UNS C17410)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 95%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R..