Polymer Property : Liquidus = 219 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 219 °C
426 °F
Nihon Superior SN97C Lead-Free Solder Alloy