Thermal Properties Metric English Comments
Liquidus 221 °C
430 °F
Indium Corp. Indalloy® 121 Sn-Ag Solder Alloy
Binary solder has history of use, marginal wetting. Standard tin-silver eutectic solder with wide application when lead-based solders do not meet temperature, strength or safety requirements. Not r..
Liquidus 221 °C
430 °F
Flow Point
Lucas-Milhaupt Clean & Bright & Brite Tin/ Silver Solder
Characteristics:This alloy is considered to be high strength solders. It has much higher creep strengths than the tin/lead solders. It is a good color match for stainless steel, and used with the p..
Liquidus 221 °C
430 °F
Williams Advanced Alloys WS221 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Liquidus 221 °C
430 °F
AIM 96.5Sn/3.5Ag Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.