Polymer Property : Liquidus = 248 °C
Polymer Property :
Liquidus =
248 °C
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Liquidus
248
°C
478
°F
Indium Corp. Indalloy® 264 Tin-Antimony Solder Alloy
Information provided by the manufacturer, Indium Corporation of America.