Polymer Property : Liquidus = 257 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 125 °C
257 °F
Indium Corp. Indalloy 13 Indium Solder Alloy
Information Provided by Indium Corporation
Liquidus 125 °C
257 °F
Indium Corp. Indalloy 1 Indium-Tin Solder Alloy
Fair wettability on glass, quartz, and many ceramics. Good low temperature malleability. Compensates for some CTE mismatch. Low vapor pressureInformation Provided by Indium Corporation