Thermal Properties Metric English Comments
Liquidus 1425 °C
2597 °F
Special Metals INCOLOY® Alloy 330
A nickel-iron-chromium alloy with an addition of silicon for enhanced oxidation resistance. It has good strength at high temperatures and excellent resistance to carburizing and oxidizing atmospher..