Liquidus 275 °C
527 °F
Indium Corp. Indalloy® 150 Pb-In Solder Alloy
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics..
Liquidus 275 °C
527 °F
Johnson Matthey LM10A Soft Solder/Flux
General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi..