Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 154 °C | 309 °F | |
Indium Corp. Indalloy 92 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Liquidus | 154 °C | 309 °F | |
Indium Corp. Indalloy® 2 In-Pb-Ag Solder Alloy Especially useful for soldering against gold, as leaching is minimized. Good thermal fatigue properties. Compatible with Indalloy numbers 204, 205, 206, 7, 10 and 150 in step-soldering applications... |