Polymer Property : Liquidus = 401 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 205 °C
401 °F
Indium Corp. Indalloy® 254 86.9Sn/10.0In/3.1Ag Lead-Free Solder Alloy
No Sn/In eutectic problem; potential use for flip chip assembly. Information provided by the manufacturer, Indium Corporation.
Liquidus 205 °C
401 °F
Indium Corp. Indalloy 114 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Liquidus 205 °C
401 °F
Williams Advanced Alloys WS205 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys