Polymer Property : Liquidus = 414 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Liquidus 212 °C
414 °F
Indium Corp. Indalloy 116 Tin-Lead Solder Alloy
General purpose solderInformation Provided by Indium Corporation
Liquidus 212 °C
414 °F
Williams Advanced Alloys WS212 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys