Thermal Properties Metric English Comments
Liquidus 217 °C
423 °F
Eutectic
Indium Corp. Indalloy® 241 95.5Sn/3.8Ag/0.7Cu Lead-Free Solder Alloy
Multicore promoted alloy.Information provided by the manufacturer, Indium Corporation.
Liquidus 217 °C
423 °F
Eutectic
Indium Corp. Indalloy® 246 95.5Sn/4.0Ag/0.5Cu Lead-Free Solder Alloy
Petzow (German) prior art reference makes this alloy patent-free.Information provided by the manufacturer, Indium Corporation.
Liquidus 217 °C
423 °F
Eutectic
Indium Corp. Indalloy® 252 95.5Sn/3.9Ag/0.6Cu Lead-Free Solder Alloy
Alloy of choice for general SMT assembly. NEMI promoted alloy (average composition of Indalloy #241& #246).Information provided by the manufacturer, Indium Corporation.
Liquidus 217 °C
423 °F
Indium Corp. Indalloy® 238 Sn-Au Solder Alloy
Lower temp eutectic, in the Au Sn system.Information provided by the manufacturer, Indium Corporation.
Liquidus 217 °C
423 °F
Williams Advanced Alloys WS217 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Liquidus 217 °C
423 °F
AIM CASTIN Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.