Thermal Properties Metric English Comments
Liquidus 314 °C
597 °F
Williams Advanced Alloys WS314 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Liquidus 314 °C
597 °F
Williams Advanced Alloys WS314A Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys