Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 729.4 °C | 1345 °F | |
Lucas-Milhaupt Silvaloy® A34T Brazing Alloy Silvaloy A34T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult wet metals su.. |
|||
Liquidus | 729.4 °C | 1345 °F | Flow Point |
Lucas-Milhaupt BRAZE 580 Silver Based Cadmium Free Filler Metal Characteristics:Braze 580 is a free flowing intermediate temperature cadmium-free silver brazing filler metal that exhibits an unusual ability to wet certain base metals that are difficult to braze .. |