Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 777.5 - 783.5 °C | 1432 - 1442 °F | |
PEAK Werkstoff DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |